Composite Silicone Braided Tube: Technical Specs
1. Factory Technical Capabilities
Our R&D team has 10 patents on composite braided tube materials and processes, equipped with 3-axis coordinate measuring instruments, dynamic pressure test machines and environmental aging test chambers. We can provide comprehensive technical data: pressure - temperature performance curves, braided density distribution maps, migration test reports and fatigue life analysis (≥100,000 cycles).
2. Material & Process Technical Details
Base material: High-purity silicone (Shore hardness 40-70A); braided material: Polyester fiber (tensile strength ≥8.0MPa), aramid fiber (≥28.0MPa), stainless steel wire (≥35.0MPa); molding parameters: Vulcanization temperature 160-180℃, holding time 30-120s, braiding density 80-95%. Mechanical properties: Tensile strength ≥6.5MPa, elongation ≥300%, tear strength ≥35kN/m.
3. Key Technical Performance Indicators
Temperature resistance: -60℃ to 200℃ (standard type); working pressure: 2.5-6.0MPa (varies by braided material); flame retardancy: UL-94 V0 (customizable); water resistance: IP67-IP68 (depending on structure); chemical resistance: Resistant to PH1-3 weak acids, PH11-13 weak alkalis and mineral oils; certification compliance: FDA 21 CFR 177.2600, LFGB, RoHS, USP Class VI.
4. Technical Services & Certification
Provide complete technical documents: MSDS, pressure test report, density detection report and full-set certification certificates. For custom projects, our technical team offers one-on-one consulting, providing braided material selection and wall thickness optimization suggestions to meet specific pressure, temperature and medium compatibility requirements.